    摘要:

    采用沉淀法制备了纳米氧化锌,并以它为前驱物,采用高温分解法对纳米氧化锌进行了载银改性处理,制备了载银氧化锌复合纳米粒子,考察了载银前后纳米粒子的粒径与结构。研究发现,采用沉淀法制备的纳米氧化锌尺寸较为均匀,粒径约为170 nm,分散性也较好;载银后的复合纳米粒子粒径略有增加,这来源于银在纳米氧化锌粒子外的成功包覆。

    Abstract:

    A precipitation approach is utilized to prepare nanoscale zinc oxide as precursor. Subsequently, silver loaded zinc oxide nanocomposites (ZnO/Ag) are prepared by hydrolysis method. The sample prior to silver loading and that thereafter are compared in terms of average diameter and structure. The results show the zinc oxide powder presenting good dispersity and uniform size with average diameter about 170 nm. Successful Silver coating on the parent powder increases the nanocomposites’ diameter slightly.

    参考文献
    相似文献
    引证文献
引用本文

庹 度.载银氧化锌复合纳米粒子的制备与表征[J].包装学报,2010,2(2):14-17.

复制
分享
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2010-03-12
  • 最后修改日期:
  • 录用日期:
  • 在线发布日期: 2015-10-28
  • 出版日期:
文章二维码